Service Manuals, User Guides, Schematic Diagrams or docs for : . Car Manuals Toyota Sienna 2004-2007 Approved SRM 46 introduc precauti

<< Back | Home

Most service manuals and schematics are PDF files, so You will need Adobre Acrobat Reader to view : Acrobat Download Some of the files are DjVu format. Readers and resources available here : DjVu Resources
For the compressed files, most common are zip and rar. Please, extract files with Your favorite compression software ( WinZip, WinRAR ... ) before viewing. If a document has multiple parts, You should download all, before extracting.
Good luck. Repair on Your own risk. Make sure You know what You are doing.




Image preview - the first page of the document
precauti


>> Download precauti documenatation <<

Text preview - extract from the document
IN-16    INTRODUCTION


        PRECAUTIONS FOR REPAIRING BODY
        STRUCTURE PANELS



        1.   HEAT REPAIR FOR BODY STRUCTURE
             PANELS
             Toyota prohibits the use of the heat repair method on body
             structure panels when repairing a vehicle damaged in a col-
             lision.
             Panels that have high strength and rigidity, as well as a long
             life span for the automobile body are being sought after.
             At Toyota, in order to fulfill these requirement, we use high
             tensile strength steel sheets and rust preventive steel
             sheets on the body.
             High tensile steel sheets are made with alloy additives and
             a special heat treatment in order to improve the strength.
             To prevent the occurrence of rust for a long period of time,
             the surface of the steel is coated with a zinc alloy.
             If a body structure parts are heat repaired with an acetylene
             torch or other heating source, the crystalline organization of
             the steel sheet will change and the strength of the steel
             sheet will be reduced.
             The ability of the body to resist rust is significantly lowered
             as well since the rust resistant zinc coating is destroyed by
             heat and the steel sheet surface is oxidized.


        2.   STRUCTURE PANEL KINKS
             A sharp deformation angle on the panel that cannot be re-
             turned to its original shape by pulling or hammering is
             called a kink.
             Since structure parts were designed to exhibit a 100% per-
             formance when they were in their original shape, if they are
             deformed in an accident, or if the deformed parts are re-
             paired and reused, they become unable to exhibit the same
             performance as intended in the design.
             It is necessary to replace the part where the kink has oc-
             curred.
 INTRODUCTION                                                IN-17

3.   IMPACT BEAM REPAIR
     The impact beam and bracket are necessary and important
     parts in maintaining a survival space for passengers in a
     side collision.
     For impact beam, we use special high tensile strength
     steel.
     The high tensile strength steel maintains its special crystal-
     line organization by heat treatment or alloy additives.
     Since these parts were designed to exhibit a 100% perfor-
     mance when they were in their original shape, if they are
     deformed in an accident, or if the deformed parts are re-
     paired and reused, they become unable to exhibit the same
     performance as intended in the design.
     It is necessary to replace the door assembly when impact
     beam or bracket is damaged.